Challenges for refractories in rotary kilns
The second step to address high burning zone shell temperatures is to install a thicker lining Common practice for a rotary kiln lining in North America is 220 mm 866in thickness Burning zone linings of 250 mm 984in are becoming more frequent Historically in larger diameter kilns burning zone linings as thick as 305 mm 12 in